Contact us now: Phone: +3556969696

Table

Thermal FR Composite Piping PP vs PP-FRP Piping

CriteriaThermal FR Composite Piping PP / PPH / PP-FRP Piping
PIPING VIEW
JOINING STRENGTH Socket Fusion joining system guaranteeing 100% Leak Proof element in pipesButt Fusion Joints with FRP Coating gives very poor joints and leads to highest leakages
THERMAL CONDUCTIVITY Lowest Thermal Conductivity 0.024 But/hr leading to Negligible Heat LossHigher Thermal Conductivity 0.066 Btu/hr leading to higher Heat Loss
FRICTION LOSS RELATED TO RA VALUELeast RA Value i.e. 0.1 Micron prevent Friction Loss in the pipeline6.5 Micron RA Value leads to higher Friction Loss due to rough inner surface and Butt Fusion Joints
INSULATIONSandwich Glass Fiber Reinforcement layer increases the temperature withstand capacity; in turn requires lesser insulation to prevent sweatingEven after FRP Coating, needs insulation to prevent sweating and heat loss leads to higher costing
MAINTENANCE NIL Maintenance having benefits such as Least Thermal Expansion and SaggingHigh chances of Maintenance because of leakages and higher Thermal Expansion leads to heavy maintenance
AESTHETIC PIPING VIEW Owing to Sandwich Glass Fiber Reinforcement layer, very less sagging gives nice and Aesthetic View to the pipelineHaving FRP Coating, disordering and messy view of the pipeline